  • Composition:
    1/22NM 67 RWS MERCERIZED WOOL 15 RECYCLED NYLON 10 RECYCLED POLYESTER 8 METALLIC
  • Price:
    Login visible
    Mobile purchase
Color:
(Note: There may be color differences online, and the specific color is subject to actual product)
Total Qty:
KG Available: 30.05KG
You select:
1KG
Lot no:
Buy Add cart Arrival notice
  • Product details
  • Washing instruction
1/22NM 67 RWS MERCERIZED WOOL 15 RECYCLED NYLON 10
FY6301S
应用
1. 12 针横机,1 根进线
2. 克重:156克/平方米
3. 抗起球标准:7200转(相同花型.针型.张力)为2-3级
4. 染色工艺:散毛染色
5. 起订量:大货:300kg/色;样纱:30kg/色
6. 参考分色卡:AUDREY
APPLICATION
1. Flat Knitting machines 12 gauge 1 ply
2. Weight per square meter:gr156(on collection fabric on jersey stitch)
3. Pilling grade:2-3:has been tested on the collection swatch(same stitch/gauge/tension)according to Pilling box(ISO 12945-1/GB/T4802.3) at 7200 turns
4. DYEING PROCESS:Fiber dye
5. MINIMUN:The minimum for Fibre dye is 30kgs(sample) and 300kgs(bulk) per colour.
6. For further colors please refer to AUDREY color card
织造:
1.纱线已打蜡,非必要勿回倒,如需回倒请联系技术部。
2.织片会有拉毛不匀造成的粗细毛,织片时请调整好张力,建议连片编织。
3.成衣如需织复杂花型组织,可能会有破洞,建议提前试样。
4.洗涤过程不宜偏酸或偏碱,PH值6.5-8效果最好,最好是中性注意去污的助剂,金银丝遇酸碱要变色的。
5.织造损耗率8%,涵盖粗细不匀,色差色花等导致的损耗。
6.收货后先试织,若有质量问题,15天内反馈。质量问题仅承担同等数量纱线,不负责面料织造和交货期费用。
KNITTING:
1:The yarn is waxed. Do not re-spool unless necessary. If re-spooling is required, please contact our technical department in advance.
2:Uneven fluffing may cause inconsistent thickness fluff on knitted pieces. Please adjust the tension properly during knitting, and it is recommended to knit them continuously in one piece.
3:If the garment requires complex pattern knitting, holes may occur. Please conduct trial knitting in advance.
4:The washing process should not be too acidic or alkaline. A pH value of 6.5 to 8 yields the best results, and neutral detergent auxiliaries are preferred. Gold and silver threads will discolor when exposed to acids or alkalis.
5:During knitting, the standard wastage rate is 8%, covering losses caused by uneven yarn count, color difference, uneven dyeing, etc.
6:After receiving the goods, conduct a trial knitting first. If there are any quality issues, please provide feedback within 15 days. In case of quality problems, we will only be responsible for providing the same quantity of yarn, and we will not cover the costs of fabric knitting and delivery time.
工业洗涤指示:
1.30℃左右温水洗涤,加入柔软剂、毛松剂,轻柔滚洗 7 分钟
2.熨烫温度小于110℃
3.平铺晾干不可滚烘
4.不可氯漂
5.不同洗衣机机型可能导致绒感效果略有差异,请根据自身需求的绒感状态调整洗涤方法
WASHING INSTRUCTION:
1:Wash in warm water (max. 30°C) with softener and wool bulking agent, then tumble wash gently for 7 minutes.
2:Iron at a maximum sole-plate temperature of 110℃.
3:Lay flat to dry, do not tumble dry.
4:Do not use chlorine bleach.
5:Different machine types may result in slight variations in the final effect. Please adjust the washing method according to the desired fabric nap effect.
COLOR FASTNESS
(Average)
LIGHT COLOUR SMEDIUM COLOUR DARK COLOURS Standard
Change Stain Change Stain Change Stain
Dry cleaning 4 4 4 3-4 4 3 ISO 105 D01/GB/T 5711
Acid perspiration 4 4 4 3-4 4 3 ISO 104 E04/GB/T 3922
Alkaline perspiration 4 4 4 3-4 4 3 ISO 104 E04/GB/T 3922
Washing 4 4 4 3-4 3 ISO 105 C06/GB/T 12490
Dry rubbing 3-4 3-4 3-4 ISO 105 X12/GB/T 3920
Wet rubbing 4 3 3 ISO 105 X12/GB/T 3920
Light (except white color) 3-4 3-4 4 ISO 105 B02/GB/T 8427
For above points marked by *,to refer to OEKO-TEX STANDARD 100 requirements
Above data are average values coming from tests carried out in our laboratories